Analytical Services: X-Ray Powder Diffraction
Raymond P. Goehner, Siemens Corporation and Monte C. Nichols, Sandia National Laboratories
|
General Use |
|---|
|
- Identification of crystalline phases contained in unknown samples |
|
- Quantitative determination of the weight fraction of crystalline phases in multiphase materials |
|
- Characterization of solid-state phase transformations |
|
- Lattice-parameter and lattice-type determinations |
|
- Orientation of single crystals |
|
- Stereographic projections |
|
- Alignment for cutting along crystallographic planes |
|
Examples of Applications |
|
- Qualitative and quantitative analysis of crystalline phases in coal ash, ceramic powders, corrosion products, and so on |
|
- Determination of phase diagrams |
|
- Determination of pressure- and/or temperature-induced phase transformations |
|
- Quantitative analysis of solid solutions from lattice-parameter measurements |
|
- Determination of anisotropic thermal expansion |
|
Samples |
|
- Form: Crystalline solids (metals, ceramics, geological materials, and so on) |
|
- Size: For powder samples 1 mg is usually adequate |
|
- Preparation: Sometimes none; sample may require crushing to fit into the sample holder |
|
Limitations |
|
- Must be crystalline for phase identification |
|
- Identification requires existence of standard patterns: JCPDS powder diffraction file of inorganic and organic phases, NBS Crystal Data (contains lattice constants for inorganic and organic phases), and Cambridge File of Organic Single Crystal Structural Data |
|
Estimated Analysis Time |
|
- Qualitative analysis requires less than 1 h for major phases, up to 16 h for trace phase confirmation |
|
- Quantitative analysis, after a procedure is set up, requires several minutes to several hours |
|
Capabilities of Related Techniques |
|
- X-ray spectrometry, inductively coupled plasma atomic emission spectroscopy, atomic absorption spectrometry, classical wet chemical analysis: Quantitative and qualitative elemental information |
|
- Auger electron spectroscopy: Elemental and structural data on small portions of the samples |
|
- Single-crystal x-ray diffraction: Crystal structure using small single crystals |
|
- Infrared and Raman spectroscopy: Molecular structure and sometimes crystal structure |
|
- Neutron diffraction: Similar information, but can be applied in some cases in which x-ray powder diffraction fails |
Reprinted with permission of ASM International®.
News
- April 2, 2008 - Passivation featured in the latest edition of NHML's Nuts & Bolts
- April 2, 2008 - Glass Vial Sprinkler Accidents featured in the latest edition of NHML's Nuts & Bolts
- January 2008 - Passing of the hands - Tim Kenney, President/CEO acquired full ownership of New Hampshire Materials Laboratory on January 8, 2008. Senior Scientist, Fred Hochgraf remains an active participant here at NHML
- January 18, 2008 - Important Customer Notice: For your convenience NHML now accepts American Express, Discover Card, MasterCard & Visa.
- October 5, 2007 - Testing for Toxic Lead May Not Be Your Only Concern
- May 21, 2007 - Embrittlement of Steels featured in NHML's Nuts&Bolts newsletter
- December 20, 2006 - NHML launches new Web site
- May 1, 2006 - Hydrolysis of Fiberglass featured in the latest edition of NHML's Nuts & Bolts
Related Materials
- Chemical Testing and Analysis
- Failure Analysis
- Mechanical Testing and Analysis
- Metallography
- Professional Services